What PSI are you guys running while sandblasting slides for cerakote.
6/3/2015 10:31:18 PM EDT
[#1]









Grit blast the parts with #100 to #120 grit aluminum oxide or garnet sand at 80 to 100 psi. Lightly blast (30-40 psi) non-metal parts such as: wood, fiberglass, plastic or polymer. For anodized aluminum parts, set the blasting pressure to 30-40 psi. Strive for an even blast pattern over the surface of the part.



This is right off Cerakote's website
for the H series
 
6/3/2015 10:33:09 PM EDT
[#2]
Metal parts 80 psi,non-metal 30 psi.
6/4/2015 1:05:48 AM EDT
[#3]
Quote History
Quoted:
Metal parts 80 psi,non-metal 30 psi.
View Quote


This is good.  Make sure and research the media you're using.  They're not all the same.  120 grit aluminum oxide is my preference.
6/5/2015 12:03:25 AM EDT
[#4]
Quote History
Quoted:



Grit blast the parts with #100 to #120 grit aluminum oxide or garnet sand at 80 to 100 psi. Lightly blast (30-40 psi) non-metal parts such as: wood, fiberglass, plastic or polymer. For anodized aluminum parts, set the blasting pressure to 30-40 psi. Strive for an even blast pattern over the surface of the part.


This is right off Cerakote's websitefor the H series  
View Quote


FYI, same for C-series.